| Properties |
Test Method |
Unit |
Specs |
| Nominal GSM |
TAPPI 410 OM-2 & ISO 536:1995 |
GSM |
170 & 176 |
| Substance Tolerance (Avg.) |
TAPPI 410 OM-2 & ISO 536:1995 |
GSM |
±2.5% |
| Bulk (Min.) |
TAPPI 411 OM-97 & ISO 534:1988 |
cc/g |
1.30 |
| Brightness (Min.) |
TAPPI 525 OM-02 & ISO 2470:1999 |
%, ISO |
84 |
| Bendsten Smoothness, TS |
TAPPI 538 OM-88 & ISO 5636-3:1992 |
|
600-1000 |
| Glazed Side, WS |
|
150-250 |
| Breaking Length (Min.), MD |
TAPPI 404 OM-87 & ISO 1924-1:1992 |
meters |
5200 |
| CD |
meters |
3000 |
| Stretch, MD/CD |
-do- |
% |
1.9/3.4 |
| Burst Factor (Min.) |
TAPPI 403 OM-02 & ISO 2758:2001 |
|
22 |
| Tear Factor (Min.) |
TAPPI 414 OM-98 & ISO 1974:1990 |
|
110 |
| Double Folds (Min.), MD/CD |
ISO 5626:1993 |
Nos |
50/20 |
| Stiffness (Min.), MD/CD |
TAPPI 489 OM-99 & ISO 2493:1992 |
Taber |
25/15 |
| Cobb (60 Sec. - Max) |
TAPPI 441 OM-98 & ISO 535:1991 |
GSM |
25 |