| Properties |
Test Method |
Unit |
Specs |
| Nominal GSM |
TAPPI 410 OM-2 & ISO 536:1995 |
GSM |
180 – 250 |
| Substance Tolerance (Avg.) |
TAPPI 410 OM-2 &
ISO 536:1995 |
GSM |
±2.5% |
| Bulk (Min.) |
TAPPI 411 OM-97 & ISO 534:1988 |
cc/g |
1.02 |
| Brightness (Min.) |
TAPPI 525 OM-02 & ISO 2470:1999 |
%ISO |
90 |
| Bendsten Smoothness, TS |
TAPPI 538 OM-88 & ISO 5636-3:1992 |
ml/min |
40-60 (180 to 220 gsm)
60-120 (230 to 250 gsm) |
| WS |
ml/min |
100-150 (180 to 220 gsm)
120-180 (230 to 250 gsm) |
| Breaking Length (Min.), MD |
TAPPI 404 OM-87 & ISO 1924-1:1992 |
meters |
3000 |
| CD |
meters |
2000 |
| Burst Factor (Min.) |
TAPPI 403 OM-02 & ISO 2758:2001 |
|
12 |
| Cobb (60 Sec. - Max) |
TAPPI 441 OM-98 & ISO 535:1991 |
GSM |
25 |